AboutEditorial BoardFor AuthorsScientific Reports
PMC full text:
Published online 2019 Dec 10. doi: 10.1038/s41598-019-55230-7

Figure 5

The catalytic catalystic degradation behavior of TC (Experimental conditions: Catalyst loading 2.5 g, pH = 3.4), [TC]0 = 400 mg L−1, working volume = 200 mL, and its degradation behavior under O3/Catalyst system, the concentration of ozone is 40 mg/L.) (a)different forms of manganese and cerium (b) different doping amount of cerium in the catalytic system (c)different initial concentrations in catalystic system (d) Pseudo-second order kinetic behavior under different tetracycline concentration in degradation process.